BS PD IEC/TS 61244-1-2014 PDF

BS PD IEC/TS 61244-1-2014 PDF

Determination of long-term radiation ageing in polymers-Techniques for monitoring diffusion-limited oxidation

$172.72 $345.44 -50%
Publisher
isbn 9780580843112
Product Code: BS PD IEC/TS 61244-1
Stock In Stock
Published: 09/30/2014
Number of Pages: 44
File Size: 1 file, 2.5 MB

Available Options

Product Description

Determination of long-term radiation ageing in polymers-Techniques for monitoring diffusion-limited oxidation

Scope: This part of IEC TS 61244, which is a technical specification, reviews experimental techniques to quantitatively monitor the effects when oxygen is present during ageing of polymers in various environments including temperature, radiation or ultraviolet. Inhomogenous ageing effects caused by diffusion-limited oxidation are often encountered and provide theoretical equations to estimate their importance. These effects make it difficult to understand the ageing process and to extrapolate accelerated exposure to long-term conditions. It is widely known that mechanical properties degrade prior to electrical properties.These changes are consequences of chemical changes such as oxidation. In this technical specification, only mechanical or chemical monitoring techniques are of interest. This technical specification does not deal with electrical monitoring techniques. Profiling techniques to monitor diffusion-limited oxidation 2.1 General The presence of diffusion-limited oxidation effects implies that various properties related to the amount of oxidation will depend upon spatial location in the material. Thus, any technique which can profile (map) these spatial variations will allow diffusion-limited oxidation to be monitored. Since polymer geometries utilize cross-sections down to a few millimetres or less, and since diffusion-limited oxidation effects are operative over such small dimensions, a useful profiling technique has to have a resolution of at least 100 µm. An additional problem related to sensitivity is the observation that severe polymer degradation typically corresponds to less than 1 % of the polymer being oxidized. Thus, a useful profiling technique shall have reasonable resolution, good sensitivity to the small chemical changes which occur, wide applicability and relative ease of operation and analysis. A number of particularly useful techniques are briefly described in this clause. 2.2 Infra-red profiling techniques Because of the ability to provide detai

Contents:

  • FOREWORD
  • INTRODUCTION
  • Scope
  • Annex A (informative) Derivation of theoretical treatment of diffusion-limited oxidation
  • Bibliography

Be the first to write a review for this product.

Write a review

Note: HTML is not translated!
Bad           Good
BS PD IEC/TS 61244-1-2014 PDF

BS PD IEC/TS 61244-1-2014 PDF

$172.72 $345.44