Photovoltaic (PV) modules – Test methods for the detection of potential-induced degradation – Part 1-1: Crystalline silicon – Delamination
Introduction: Potential-induced degradation (PID) refers to any PV module degradation that is caused by the stress of an electric potential between the active cell circuit and the external surfaces or parts of the PV module. This part of IEC 62804 is for testing and evaluating the durability of crystalline silicon PV modules for PID in the mode of delamination (PID-d), as may be induced by the stress factors of moisture and system voltage. The applied stresses, with system voltage being the principal factor in IEC 62804-series documents, manifest themselves in different degradation modes that depend in part on the module technology. Therefore, a series of technical specifications is being developed to define PID tests for different PV module technologies and differing PID modes. IEC TS 62804-1 defines test methods for evaluating power loss by PID in crystalline silicon PV modules. IEC TS 62804-1-1 defines a test method for evaluating delamination by PID in crystalline silicon PV modules. IEC TS 62804-2 defines test methods for evaluating power loss by PID in thin-film PV modules and modules with moisture-sensitive components and moisture-barrier packaging. Additional TSs in the series may be introduced in the future for emerging module technologies, mechanisms, or evaluation methods. Delamination of PV modules is a failure mode that can lead to electrical shocks, ground faults, rapid moisture ingress or collection of condensed moisture and can be associated with corrosion, some loss in pho
Scope: This part of IEC 62804 defines procedures to test and evaluate for potential-induced degradation-delamination (PID-d) mode in the laminate of crystalline silicon PV modules— principally those with one or two glass faces. This document evaluates delamination attributable to current transfer between ground and the module cell circuit. Elements driving the delamination that this test is designed to actuate include reduced adhesion associated with damp heat exposure, sodium accumulation at interfaces, and cathodic gas evolution in the cell circuit, metallization, and other components within the PV module activated by the voltage potential. The change in power of crystalline silicon PV modules associated with the stress factors applied (the purview of IEC TS 62804-1) is not considered in the scope. Modules are tested in a climactic chamber with damp heat and application of module-rated system voltage to the cell circuit in each polarity that is specified or allowed in the module documentation. This document does not differentiate the effects of some construction methods of mitigating PID—for example, the use of rear rail mounts, edge clips, and insulating frames that may serve to electrically isolate the module faces to varying extents. The actual durability of modules to system voltage stress will depend on the mounting design and the environmental conditions under which the modules are operated. These tests are intended to assess the sensitivity of the PV module laminate to PID-d irrespective of actual stresses under operation in different climates and systems.
Contents:
- FOREWORD
- INTRODUCTION
- Scope