ASTM E399-24 PDF

ASTM E399-24 PDF

Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness of Metallic Materials

$52.00 $104.00 -50%
Product Code: ASTM E399
Stock In Stock
Published: 2024
Number of Pages: 40

Available Options

Product Description

Significance and Use
 5.1  The property K Ic determined by this test method characterizes the resistance of a material to fracture in a neutral environment in the presence of a sharp crack under essentially linear-elastic stress and severe tensile constraint, such that (1) the state of stress near the crack front approaches tritensile plane strain, and (2) the crack-tip plastic zone is small compared to the crack size, specimen thickness, and ligament ahead of the crack.
 5.1.1  Variation in the value of K Ic can be expected within the allowable range of specimen proportions, a/W and W/B . K Ic may also be expected to rise with increasing ligament size. Notwithstanding these variations, however, K Ic is believed to represent a lower limiting value of fracture toughness (for 2 % apparent crack extension) in the environment and at the speed and temperature of the test.
 5.1.2  Lower and more highly variable values of fracture toughness can be obtained from specimens that fail by cleavage fracture; for example, specimens of ferritic steels tested at temperatures in the ductile-to-brittle transition region or below. Specimens failing by cleavage are also more likely to exhibit warm prestressing effects, where precracking at a temperature higher than the test temperature can artificially increase the fracture toughness measured ( 2 ) . The present test method is not intended for cleavage fracture. Instead, the user is referred to Test Method E1921 and E1820 which are applicable to cleavage fracture and contain safeguards against warm prestressing. Likewise this test method should not be used when specimen failure is accompanied by appreciable plastic deformation even after the specimen size has been maximized within product dimensional constraints. Guidance on testing elastic-plastic materials is given in Test Method E1820 .
 5.1.3  The value of K Ic obtained by this test method may be used to estimate the relation between failure stress and crack size for a material in service wherein the conditions of high constraint described above would be expected. Background information concerning the basis for development of this test method in terms of linear elastic fracture mechanics may be found in Refs ( 1 ) and ( 3 ) .
 5.1.4  Cyclic forces can cause crack extension at K I values less than K Ic . Crack extension under cyclic or sustained forces (as by stress corrosion cracking or creep crack growth) can be influenced by temperature and environment. Therefore, when K Ic is applied to the design of service components, differences between laboratory test and field conditions shall be considered.
 5.1.5  Plane-strain fracture toughness testing is unusual in that there can be no advance assurance that a valid K Ic will be determined in a particular test. Therefore, compliance with the specified validity criteria of this test method is essential.
 5.1.6 Residual stresses can introduce bias into the indicated K Q and K Ic value determinations. The effect can be especially significant for specimens removed from as-heat treated or otherwise non-stress relieved stock, from weldments, from complex wrought products, rapidly-solidified castings, additively-manufactured products or from products with intentionally induced residual stresses. In addition, residual stresses will redistribute when the specimen is extracted from the host product and machined. The magnitude of residual stress influence on K Q and K Ic in the test specimen may be quite different from that in the original or finish machined product. In addition, the behavior of cracks in the full-sized product may not be predictable from the fracture toughness measured on the specimen because of the influence of the different residual stresses in each. Indications of residual stress include distortion during specimen machining, results that are specimen configuration dependent, and irregular fatigue precrack growth (either excessive crack front curvature or out-of-plane growth). Guide B909 provides supplementary guidelines for plane strain fracture toughness testing of aluminum alloy products for which complete stress relief is not practicable. Guide  B909 includes additional guidelines for recognizing when residual stresses may be significantly biasing test results, and methods for minimizing the effects of residual stress during testing.
 5.2  This test method can serve the following purposes:
 5.2.1  In research and development, to establish in quantitative terms significant to service performance, the effects of metallurgical variables such as composition or heat treatment, or of fabricating operations such as welding or forming, on the fracture toughness of new or existing materials.
 5.2.2  In service evaluation, to establish the suitability of a material for a specific application for which the stress conditions are prescribed and for which maximum flaw sizes can be established with confidence.
 5.2.3  For specifications of acceptance and manufacturing quality control, but only when there is a sound basis for specifying minimum K Ic values, and then only if the dimensions of the product are sufficient to provide specimens of the size required for valid K Ic determination. The specification of K Ic values in relation to a particular application should signify that a fracture control study has been conducted for the component in relation to the expected loading and environment, and in relation to the sensitivity and reliability of the crack detection procedures that are to be applied prior to service and subsequently during the anticipated life.
 Scope
 1.1  This test method covers the determination of fracture toughness ( K Ic and optionally K Isi ) of metallic materials under predominantly linear-elastic, plane-strain conditions using fatigue precracked specimens having a thickness of 1.6 mm (0.063 in.) or greater 2 subjected to slowly, or in special (elective) cases rapidly, increasing crack-displacement force. Details of test apparatus, specimen configuration, and experimental procedure are given in the annexes. Two procedures are outlined for using the experimental data to calculate fracture toughness values:
 1.1.1  The K Ic test procedure is described in the main body of this test standard and is a mandatory part of the testing and results reporting procedure for this test method. The K Ic test procedure is based on crack growth of up to 2 % percent of the specimen width. This can lead to a specimen size dependent rising fracture toughness resistance curve, with larger specimens producing higher fracture toughness results.
 1.1.2  The K Isi test procedure is described in Appendix X1 and is an optional part of this test method. The K Isi test procedure is based on a fixed amount of crack extension of 0.5 mm, and as a result, K Isi is less sensitive to specimen size than K Ic . This less size-sensitive fracture toughness, K Isi , is called size-insensitive throughout this test method. Appendix X1 contains an optional procedure for reinterpreting the force-displacement test record recorded as part of this test method to calculate the additional fracture toughness value, K Isi .
 Note 1:   Plane-strain fracture toughness tests of materials thinner than 1.6 mm (0.063 in.) that are sufficiently brittle (see 7.1 ) can be made using other types of specimens ( 1 ) . 3 There is no standard test method for such thin materials.
 1.2  This test method is divided into two parts. The first part gives general recommendations and requirements for testing and includes specific requirements for the K Ic test procedure. The second part consists of Annexes that give specific information on displacement gage and loading fixture design, special requirements for individual specimen configurations, and detailed procedures for fatigue precracking. Additional annexes are provided that give specific procedures for beryllium and rapid-force testing, and the K Isi test procedure, which provides an optional additional analysis procedure for the test data collected as part of the K Ic test procedure.
 1.3  General information and requirements common to all specimen configurations:
 Section
 Referenced Documents
 2
 Terminology
 3
  Stress-Intensity Factor
 3.1.1
  Plane-Strain Fracture Toughness
 3.1.2
  Crack Plane Orientation
 3.1.4
 Summary of Test Method
 4
 Significance and Use
 5
  Significance
 5.1
  Precautions
 5.1.1 – 5.1.5
  Practical Applications
 5.2
 Apparatus (see also 1.4 )
 6
  Tension Machine
 6.1
  Fatigue Machine
 6.2
  Loading Fixtures
 6.3
  Displacement Gage, Measurement
 6.4
 Specimen Size, Configurations, and Preparation (see also 1.5 )
 7
  Specimen Size Estimates
 7.1
  Standard and Alternative Specimen Configurations
 7.2
  Fatigue Crack Starter Notches
 7.3.1
  Fatigue Precracking (see also 1.6 )
 7.3.2
  Crack Extension Beyond Starter Notch
 7.3.2.2
 General Procedure
 8
  Specimen Measurements
   Thickness
 8.2.1
   Width
 8.2.2
   Crack Size
 8.2.3
   Crack Plane Angle
 8.2.4
  Specimen Testing
   Loading Methods
 8.3
   Loading Rate
 8.4
   Test Record
 8.5
 Calculation and Interpretation of Results
 9
  Test Record Analysis
 9.1
   P m a x /P Q  Validity Requirement
 9.1.3
  Specimen Size Validity Requirements
 9.1.4
 Reporting
 10
 Precision and Bias
 11
 1.4  Specific requirements related to test apparatus:
 Double-Cantilever Displacement Gage
 Annex A1
 Testing Fixtures
 Annex A2
 Bend Specimen Loading Fixture
 Annex A2.1
 Compact Specimen Loading Clevis
 Annex A2.2
 1.5  Specific requirements related to individual specimen configurations:
 Bend Specimen SE(B)
 Annex A3
 Compact Specimen C(T)
 Annex A4
 Disk-Shaped Compact Specimen DC(T)
 Annex A5
 Arc-Shaped Tension Specimen A(T)
 Annex A6
 Arc-Shaped Bend Specimen A(B)
 Annex A7
 1.6  Specific requirements related to special test procedures:
 Fatigue Precracking K Ic and K Isi Specimens
 Annex A8
 Hot-Pressed Beryllium Testing
 Annex A9
 Rapid-Force Testing
 Annex A10
 Determination of K Isi
 Appendix X1
 1.7  The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.
 1.8   This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
 1.9   This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Be the first to write a review for this product.

Write a review

Note: HTML is not translated!
Bad           Good
ASTM E399-24 PDF

ASTM E399-24 PDF

$52.00 $104.00