Iron ores. Determination of loss on ignition. Non-oxidised ores
Scope: This Technical Report describes a gravimetric method for the determination of the loss in mass of non- oxidized iron ores, when ignited at 1 000 °C. This method is applicable to a concentration range of a mass fraction of −3,0 % to 7,0 % loss on ignition in natural iron ores, iron ore concentrates and agglomerates, and sinters. The method is not applicable to the following: a) processed ores containing metallic iron (direct reduced iron); b) natural or processed ores in which the sulfur content is higher than a mass fraction of 0,2 %; c) internationally traded ores with combined water greater than 2,5 %. NOTE 1 Loss on ignition can be used as an estimate of combined water. NOTE 2 This method is intended for in-house use and is not intended for referee purposes. 2 Principle A test portion is heated in a muffle furnace at 1 000 °C for 60 min and cooled in a desiccator. The decreased mass of the test portion is then measured. 3 Reagents During the analysis, use only reagents of recognized analytical grade. 3.1 Silica gel, dried at 105 °C for 4 h. 4 Apparatus Ordinary laboratory apparatus and the following: 4.1 Silica, porcelain or platinum crucibles, 15 ml to 25 ml capacity, with lids. The crucibles should be pre-conditioned in the muffle furnace at 1 000 °C for 60 min. Crucibles and lids should be stored in the desiccator (4.4) prior to use. If platinum crucibles used for LOI analysis are to be used for flux fusions, platinum ware should be thoroughly cleaned to prevent cross-contamination. 4.2 Balance, capable of reading to the nearest 0,1 mg at the mass load of the crucible. TECHNICAL REPORT ISO/TR 18230:2015(E)