Superconductivity – Part 18: Mechanical properties measurement – Room temperature tensile test of Ag- and/or Ag alloy-sheathed Bi-2223 and Bi-2212 composite superconductors
Introduction: Several types of composite superconductors have now been commercialised. Especially, high temperature superconductors such as Ag- and/or Ag alloy-sheathed Bi-2223 (Ag/Bi-2223) and Ag- and/or Ag alloy-sheathed Bi-2212 (Ag/Bi-2212) wires are now manufactured in industrial scale. Commercial composite superconductors have a high current density and a small cross-sectional area. The major applications of composite superconductors are to build electrical power devices and superconducting magnets. While the magnet is being manufactured, complicated stresses/strains are applied to its windings and, while it is being energized, a large electromagnetic force is applied to the superconducting wires because of its high current density. It is therefore indispensable to determine the mechanical properties of the superconductive wires from which the windings are made. The Ag/Bi-2223 and Ag/Bi-2212 superconductive composite wires fabricated by the powder-in -tube method are composed of a number of oxide filaments with silver and silver alloy as a stabilizer and supporter. In the case that the external reinforcement of Ag/Bi-2223 and Ag/Bi-2212 wires by using thin stainless or Cu alloy foils has been adopted in order to resist the large electromagnet force, this standard shall be also applied.
Scope: This International Standard specifies a test method detailing the tensile test procedures to be carried out on Ag/Bi-2223 and Ag/Bi-2212 superconductive composite wires at room temperature. This test is used to measure the modulus of elasticity and to determine the 0,2 % proof strength. When the 0,2 % proof strength could not be determined due to earlier failure, the stress level at apparent strains of 0,05 %, 0,1 %, 0,15 %, 0,2 %, 0,25 % with increment of 0,05 % is measured. The values for elastic limit, fracture strength, percentage elongation after fracture and the fitted type of 0,2 % proof strength serve only as a reference (see Clauses A.4, A.5, A.6 and A.10). The sample covered by this test procedure should have a round or rectangular cross-section with an area of 0,3 mm2 to 2,0 mm2 (corresponding to the tape-shaped wires with width of 2,0 mm to 5,0 mm and thickness of 0,16 mm to 0,4 mm).
Contents:
- Scope
- 10 Test report
- 10.1 Specimen
- 10.2 Results
- 10.3 Test conditions