IEC TS 61244-1-2014 PDF

IEC TS 61244-1-2014 PDF

Determination of long-term radiation ageing in polymers-Part 1: Techniques for monitoring diffusion-limited oxidation

$186.00 $371.99 -50%
Product Code: IEC TS 61244-1
Stock In Stock
Edition: 2.0
Published: 08/2014
Number of Pages: 90
File Size: 1 file, 1 Byte

Available Options

Product Description

Determination of long-term radiation ageing in polymers – Part 1: Techniques for monitoring diffusion-limited oxidation

Introduction: It is usually necessary to estimate the anticipated lifetime of a polymeric material in various usage environments. For extended lifetimes (years), this often requires the application of accelerated ageing techniques which typically involve the modelling of results obtained at higher-than-ambient environmental stress levels. For many practical applications, air is present during environmental exposures – this usually implies that important oxidation effects underlie the degradation of the material. Unfortunately, exposure of polymers to air during ageing often results in inhomogeneously oxidized samples, a complication which affects attempts both to understand the oxidation process and to extrapolate accelerated exposures to long-term conditions. The most important inhomogeneous oxidation complication involves diffusion-limited oxidation. The significance of this complication in various environments, including thermal [1] 1 radiation [2 to 4] and ultraviolet [5] has been recognized for many years. Diffusion-limited oxidation can occur whenever the rate of oxygen consumption in a material is greater than the rate at which oxygen can be resupplied to the interior of the material by diffusion processes from the surrounding air atmosphere. Such instances result in a smooth drop in the oxygen concentration from its equilibrium sorption value at the sample surfaces to a diminished or non-existent value in the sample interior. This will usually lead to a heterogeneity in the oxidati

Scope: This part of IEC TS 61244, which is a technical specification, reviews experimental techniques to quantitatively monitor the effects when oxygen is present during ageing of polymers in various environments including temperature, radiation or ultraviolet. Inhomogenous ageing effects caused by diffusion-limited oxidation are often encountered and provide theoretical equations to estimate their importance. These effects make it difficult to understand the ageing process and to extrapolate accelerated exposure to long-term conditions. It is widely known that mechanical properties degrade prior to electrical properties.These changes are consequences of chemical changes such as oxidation. In this technical specification, only mechanical or chemical monitoring techniques are of interest. This technical specification does not deal with electrical monitoring techniques. Profiling techniques to monitor diffusion-limited oxidation 2.1 General The presence of diffusion-limited oxidation effects implies that various properties related to the amount of oxidation will depend upon spatial location in the material. Thus, any technique which can profile (map) these spatial variations will allow diffusion-limited oxidation to be monitored. Since polymer geometries utilize cross-sections down to a few millimetres or less, and since diffusion-limited oxidation effects are operative over such small dimensions, a useful profiling technique has to have a resolution of at least 100 µm. An additional problem related to sensitivity is the observation that severe polymer degradation typically corresponds to less than 1 % of the polymer being oxidized. Thus, a useful profiling technique shall have reasonable resolution, good sensitivity to the small chemical changes which occur, wide applicability and relative ease of operation and analysis. A number of particularly useful techniques are briefly described in this clause. 2.2 Infra-red profiling techniques Because of the ability to provide detailed chemical information on thin film samples, infra-red spectroscopy has been used to monitor diffusion-limited oxidation effects for more than 25 years [17]. Any oxidation-sensitive infra-red peak t

Contents:

  • FOREWORD
  • INTRODUCTION
  • Scope
  • 100 °C (from [18])