Photovoltaic (PV) modules – Test methods for the detection of potential-induced degradation – Part 2: Thin-film
Introduction: Potential-induced degradation (PID) refers to any PV module degradation that is caused by the stress of an electric potential between the active cell circuit and the external surfaces or parts of the PV module. The applied stresses, with system voltage being the principal factor in IEC 62804 series documents, manifest themselves in different degradation modes that depend in part on the module technology. Therefore, a series of technical specifications is being developed to define PID tests for different PV module technologies and differing PID modes. IEC TS 62804-1:2015, Photovoltaic (PV) modules – Test methods for the detection of potential- induced degradation – Part 1: Crystalline silicon defines test methods for evaluating power loss by PID in crystalline silicon PV modules. IEC TS 62804-1-1:2020, Photovoltaic (PV) modules – Test methods for the detection of potential- induced degradation – Part 1-1: Crystalline silicon – Delamination defines a test method for evaluating delamination by PID associated with electrochemical processes in crystalline silicon PV modules. This part of IEC 62804 defines test methods for evaluating power loss by PID in thin-film PV modules with moisture sensitive components and those which use moisture barrier encapsulation because of such sensitivity. A future document will be required for evaluating corrosion and delamination associated with electrochemical processes in thin-film PV modules and modules with moisture sensitive components with mo
Scope: This part of IEC 62804 defines apparatus and procedures to test and evaluate the durability of photovoltaic (PV) modules to power loss by the effects of high voltage stress in a damp heat environment, referred to as potential-induced degradation (PID). This document defines a test method that compares the coulomb transfer between the active cell circuit and ground through the module packaging under voltage stress during accelerated stress testing with the coulomb transfer during outdoor testing to determine an acceleration factor for the PID. It is designed for thin-film PV modules and modules containing moisture sensitive films protected by vapour barrier packaging, principally with one or two glass surfaces. This document tests for the degradation mechanisms involving mobile ions influencing the electric field over the semiconductor absorber layer or electronically interacting with the films such that module power is affected. This document does not specifically test for electrochemical corrosion or delamination associated with application of system voltage. This document does not contain pass or fail criteria and it is not intended for design qualification. The procedures contained herein, with testing in chamber in combination with in the field or testing in the field alone are intended for use when it is desired to quantify the acceleration provided by the applied stress levels over regular use conditions in the natural environment using coulombs transferred between the module and ground as the index for damage incurred by PID. The procedures for quantifying the acceleration are not recommended when coulombs transferred are not an indicator of damage by PID to the module. The procedures are not directly applicable when moisture ingress into the module laminate occurs affecting PID rate, and to the extent that there is power recovery when the factor of system voltage bias is removed after correctly applying the procedures herein, within the period of testing. The protocols given herein give results according to the chamber stress levels applied and the module grounding configuration used in the test. Because the stress method of testing in an environmental c
Contents:
- FOREWORD
- INTRODUCTION
- Scope