Caoutchouc vulcanisé ou thermoplastique - Estimation de la durée de vie et de la température maximale d’utilisation

Introduction: The rate of a chemical reaction normally increases with increasing temperature. By exposing test pieces to a series of elevated temperatures, the relation between the rate of degradative mechanisms and temperature can be deduced. Estimates can then be made by extrapolation, for a given temperature, of the degree of degradation after a given time or the time required to reach a given degree of degradation. The reaction rate-temperature relationship can often be represented by the Arrhenius equation. The reaction rate at any given temperature is obtained from the change in the value of a selected property with exposure time at that temperature. The reaction rate can be represented by the time to a particular degree of degradation (threshold value) and can be the only practical measure if the property-temperature relation is complex. The Arrhenius approach is only suitable for chemical degradation reactions and can give incorrect results for tests where physical (viscoelastic) changes cannot easily be separated from chemical changes. An alternative approach for rubbers is to use the Williams Landel Ferry (WLF) equation. This equation performs a time-temperature transformation, and no assumptions are made as to the form of the property-time relation at any temperature. Hence, in principle, it can be applied to any physical property, including set and relaxation, or where the property/time relation is complex. Further explanation of the use of the WLF equation can be found in Refe

Scope: This document specifies the principles and procedures for estimating the thermal endurance of rubbers from the results of exposure to elevated temperatures for long periods. Two approaches are specified (see Introduction): — one using the Arrhenius equation; — the other using the WLF equation. In this document, the estimation of thermal endurance is based solely on the change in selected properties resulting from periods of exposure to elevated temperatures. The various properties of rubbers change at different rates on thermal ageing, hence comparison between different rubbers can only be made using the same properties.