Steel and iron castings — Visual testing of surface quality
Introduction: The surface roughness of a casting is influenced by the manufacturing process (moulding, grinding, finishing, etc.), the moulding materials used (sand, coating, etc.), the equipment available and the alloy cast. Since cast surfaces do not exhibit the same cyclic regularity as machined surfaces, it is difficult to evaluate their roughness using conventional mechanical, optical, or pneumatic devices. The use of visual/tactile comparators is therefore preferred in these circumstances. Moreover, in order to take account of the irregularities on as-cast surfaces, ground surfaces or other means of finishing of castings, comparators should have relatively large dimensions (greater than or equal to 15 000 mm2) in order to make them more reliable and their results repeatable and consistent. Two sets of comparators1) are in widespread use: 1. SCRATA or CTI comparators for the definition of surface quality of steel castings, available from Castings Technology International (CTI), Advanced Manufacturing Park, Brunel Way, Rotherham, South Yorkshire, United Kingdom, info@castingstechnology.com; 2. BNIF 359, Recommandation technique du Bureau de Normalisation des Industries de la Fonderie. Caractérisation d'états de surface des pièces moulées — Utilisation des échantillons types de 110 × 160 mm, available from CTIF, 44 avenue de la Division Leclerc, 92310 Sèvres, France, www.ctif -editions.com. 1) This information is given for the convenience of users of this document and does not cons
Scope: 1.1 This document covers the acceptance criteria for the visual testing of the surface of steel and iron castings. 1.2 Acceptance levels utilize Bureau de Normalisation des Industries de la Fonderie (BNIF) and Steel Castings Research and Trade Association (SCRATA) or Casting Technology International (CTI) reference comparators for the visual determination of surface roughness and surface discontinuities described as follows: — surface roughness; — thermal dressing; — mechanical dressing; — non-metallic inclusions; — gas porosity; — fusion discontinuities; — expansion discontinuities; — metal inserts.