Metallic materials - Fatigue testing - Fatigue crack growth method
Introduction: This document is intended to provide specifications for generation of fatigue crack growth rate data. Test results are expressed in terms of the fatigue crack growth rate as a function of crack-tip stress- intensity factor range, ΔK, as defined by the theory of linear elastic fracture mechanics[15][16][17] [18][19][20]. Expressed in these terms, the results characterize a material's resistance to subcritical crack extension under cyclic force test conditions. This resistance is independent of specimen planar geometry and thickness, within the limitations specified in Clause 6. This document describes a method of subjecting a precracked notched specimen to a cyclic force. The crack length, a, is measured as a function of the number of elapsed force cycles, N. From the collected crack length and corresponding force cycles relationship, the fatigue crack growth rate, da/dN, is determined and is expressed as a function of stress-intensity factor range, ΔK. Materials that can be tested by this method are limited by size, thickness and strength only to the extent that the material remains predominantly in an elastic condition during testing and that buckling is precluded. Specimen size can vary over a wide range. Proportional planar dimensions for six standard configurations are presented. The choice of a particular specimen configuration can be dictated by the actual component geometry, compression test conditions or suitability for a particular test environment. Specimen size is
Scope: This document describes tests for determining the fatigue crack growth rate from the fatigue crack growth threshold stress-intensity factor range, ΔKth, to the onset of rapid, unstable fracture. This document is primarily intended for use in evaluating isotropic metallic materials under predominantly linear-elastic stress conditions and with force applied only perpendicular to the crack plane (mode I stress condition), and with a constant force ratio, R.