Fibre-reinforced plastic composites — Determination of open-hole compression strength
Introduction: In preparing this document, reference has been made to other similar open-hole compression methods (JIS K 7093[1], ASTM D6484/D6484M-09[2]) and related methods, i.e. open-hole tension in ASTM D5766/ D5766M6[3] and pin-bearing in ISO 12815[4]. The scope covers all current and future fibre-reinforced plastic composites meeting the requirements of this document. This document incorporates three methods that have different suitability and do not necessarily yield identical properties. All the methods use the maximum load to define the open-hole compressive strength. © ISO 2025 – All rights reserved
Scope: This document specifies the test method to determine the open-hole compressive strength of laminated fibre-reinforced plastic composites. The laminate is intended to be a balanced and symmetrical lay-up or be otherwise homogeneous through the thickness. This document applies to all textile diameter fibre types (carbon, glass, aramids, etc.) and matrices (e.g. thermoset, thermoplastic) that meet the requirements of this document. This document includes three methods: — method 1 (short specimen with support fixture); — method 2 (short specimen without support fixture); — method 3 (long specimen with support fixture as in ASTM D6484/D6484M-09, methods A and B). Method 1 employs an L-shaped base fixture and two end fixtures. These end fixtures are compressed between the platens of the test machine. Method 2 employs end supports similar to the fixtures given in ISO 14126:2023, D.1. This method is useful for cyclic loading conditions test, including under fully or partly reversed loading conditions when the specimen is clamped by hydraulic grips without support fixtures Method 3 has two types of loading methods, i.e. 3A and 3B. In method 3A, the specimen is placed within a stabilization fixture, which is then clamped by hydraulic grips. In method 3B, the specimen is placed within a stabilization fixture and then end-loaded by platens. Full details of test methods 3A and 3B are given in ASTM D6484/D6484M-09, procedure A and procedure B, respectively. NOTE Specimen configurations and force introduction varies for the three methods covered within this document. Results obtained using methods 1, 2 and 3 might not be equivalent for all laminates in all environments.