Plastiques - Détermination de la ténacité à la rupture (GIC et KIC) - Application de la mécanique linéaire élastique de la rupture (LEFM)
Introduction: This document is based on a testing protocol developed by the European Structural Integrity Society (ESIS), Technical Committee 4, Polymers, Polymer Composites and Adhesives, who carried out the preliminary enabling research through a series of round-robin exercises which covered a range of material samples, specimen geometries, test instruments and operational conditions. This activity involved nearly 10 laboratories from different countries. See References [1] and [3]. © ISO 2018 – All rights reserved
Scope: This document specifies the principles for determining the fracture toughness of plastics in the crack- opening mode (mode I) under defined conditions. Two test methods with cracked specimens are defined, namely three-point-bending tests and compact-specimen tensile tests in order to suit different types of equipment available or different types of material. The methods are suitable for use with the following range of materials, including their compounds containing short fibres of the length ≤ 7,5 mm: — rigid and semi-rigid thermoplastic moulding, extrusion and casting materials; — rigid and semi-rigid thermosetting moulding and casting materials. In general, short fibre lengths of 0,1 mm to 7,5 mm are known to cause heterogeneity and anisotropy in the crack tip fracture process zone. Therefore, where relevant, Annex B offers some guidelines to extend the application of the same testing procedure, with some reservations, to rigid and semi-rigid thermoplastic or thermosetting plastics containing such short fibres. Certain restrictions on the linearity of the load-displacement diagram, on the specimen width and on the thickness are imposed to ensure validity (see 6.4) since the scheme used assumes linear elastic behaviour of the cracked material and a state of plane strain at the crack tip. Finally, the crack needs to be sharp enough so that an even sharper crack does not result in significantly lower values of the measured properties.