Polyethylene (PE) materials for piping systems - Determination of resistance to slow crack growth under cyclic loading - Cracked Round Bar test method
Introduction: Knowledge about the resistance to long-term failure mechanisms as a result of crack initiation and slow crack growth (SCG) is important for the ranking and pre-selection of thermoplastic materials, especially for long-term applications such as pipes and fittings made of polyethylene. Several tests to determine the relevant failure mechanisms are available today where elevated temperatures and also the combination with stress cracking liquids are used to decrease the time frame for testing. However, developments in modern raw materials have led to a significant increase of resistance of polyethylene to crack initiation and SCG so that testing with available methods exceeds practical time frames. Therefore, new acceleration methods, preferably at application relevant temperatures and without additional time reducing liquids, are required. This test method achieves a significant decrease of testing time even at ambient temperatures of 23 °C. This is more relevant to the temperature range of many applications and testing at this temperature does not change the structural status of the polymer. Acceleration of material testing is achieved by the specimen geometry and the cyclic loading regime to result in completion of testing in a relatively short time.[2],[3],[4] © ISO 2015 – All rights reserved
Scope: This International Standard specifies a method to determine the resistance to slow crack growth (SCG) of polyethylene materials, pipes, and fittings. The test is applicable to samples taken from compression moulded sheet or extruded pipes and injection moulded fittings of suitable thickness. This International Standard provides a method that is suitable for an accelerated fracture-mechanics characterization at ambient temperatures of 23 °C of different polyethylene grades, especially for PE 80 and PE 100 types for pipe applications. NOTE This test method could be adapted for other thermoplastics materials by developing the procedure using different test parameters.