Metallic materials — Fatigue testing — Axial force-controlled method
Introduction: This document is intended to provide requirements and guidance for conducting axial, constant-amplitude, force-controlled, cyclic fatigue tests on specimens of a metal for the sake of generating fatigue-life data (i.e. stress vs. cycles to failure) for material characterization. Nominally identical specimens are mounted in an axial force-type fatigue-testing machine and subjected to the required cyclic force conditions that introduce any one of the types of cyclic stress as illustrated in Figure 1. The test waveform should be of constant amplitude and sinusoidal unless otherwise specified. The force being applied to the specimen is along the longitudinal axis passing through the centroid of each cross-section. The test is continued until the specimen fails or until a predetermined number of stress cycles have been exceeded (see Clauses 4 and 10). Tests are typically conducted at ambient temperature (ideally between 10 °C to 35 °C). NOTE The results of a fatigue test can be affected by atmospheric conditions and where controlled conditions are required, ISO 554:1976, 2.1 applies. Caution should be taken regarding the selected test temperature of such isothermal testing so that there are no possible phase changes in the material's microstructure. At elevated temperature creep phenomena can occur. It is recommended to maintain the test temperature, T, at ≤ 0,3 of the melting temperature, Tm, of the material being tested, i.e. the homologous temperature defined as: Th = T(K)/Tm(K
Scope: This document specifies the conditions for conducting axial, constant-amplitude, force-controlled, fatigue tests at ambient, elevated, and low temperature on metallic specimens, without deliberately introduced stress concentrations. The object of testing while employing this document is to provide fatigue information, such as the relation between applied stress and number of cycles to failure for a given material condition, such as microstructure, at various stress ratios. While the form, preparation and testing of specimens of circular and rectangular cross-section are described, component testing and other specialized forms of testing are not included in this document. NOTE 1 Fatigue tests on notched specimens are not covered by this document since the shape and size of notched test pieces have not been standardized. However, fatigue-test procedures described in this document can be applied to fatigue tests of such notched specimens. NOTE 2 Throughout this document, the engineering stress is employed. Engineering stress is equal to the axially applied force divided by the cross-sectional area of the test specimen, S = Force/Area, [MPa], at the test temperature.