Plastiques - Détermination de la fissuration sous contrainte dans un environnement donné (ESC) du polyéthylène - Essai sur éprouvette entièrement entaillée (FNCT)
Introduction: Since mid-2000, the full-notch creep test (FNCT) has been widely used as one of the tests characterizing the environmental stress cracking (ESC) of polyethylene (PE) materials used in demanding applications. Among current ESC tests, the FNCT is relatively simple, easy to perform and still a sensitive laboratory scale test method to characterize ESC resistance of PE materials. The advantage of FNCT is that it enables the evaluation of the whole PE product range by variation of test conditions (test specimen geometry, temperature, medium and load conditions). The FNCT method was standardized in 2004 as a PE material property, with partial precision statement based on the repeatability for a 6 mm × 6 mm-cross-sectional test specimen (Type B). Since then, several interlaboratory tests have been performed, resulting in a repeatability statement for 10 mm × 10 mm- cross-sectional test specimen (Type A). Type A specimen is prepared by using modified compression moulding conditions, which give more consistent test results compared to the original moulding conditions. In addition, due to recent development of new PE pipe materials, known as PE 100 RC, which exhibit substantially improved crack resistance, it became necessary to define test conditions for these materials. Testing of these materials using the conditions specified in the previous edition of this document (i.e. ISO 16770:2004) resulted in failure times of one year or longer. As a consequence, this document includes extend
Scope: This document specifies a method for determining the environmental stress cracking (ESC) resistance of polyethylene (PE) materials in a defined test environment. The test is carried out on notched test specimens machined from moulded sheets/specimens or from finished products. The test specimen is subjected to a static tensile load when immersed into an environment such as a surfactant solution held at a specified temperature. The time to failure is measured. The method has been specifically developed for polyethylene materials but can be used to evaluate PE products, such as pipes, fusion welds/fittings and blow-moulded PE containers to study the effect of aggressive environments, i.e. dangerous goods and chemicals. The method is suitable for use with test specimens moulded to chosen dimensions or machined from compression moulded sheets or injection moulded specimens, or from finished products, such as mouldings and pipes. When the test specimens are machined from extruded or moulded parts, the results can be affected not only by properties of the material, but also by stresses or orientation introduced during processing.