Nanotechnologies — Positron annihilation lifetime measurement for nanopore evaluation in materials
Introduction: This document describes a method for measuring and reporting the lifetime of ortho-positronium utilizing the positron annihilation lifetime technique. Some of the positrons introduced into insulating materials, like oxides and organic polymers, can form the spin parallel positron-electron bound state ortho-positronium, which tends to localize in voids. In its trapped state, ortho-positronium annihilates with a lifetime that is less than its intrinsic lifetime of 142 ns in vacuum via a two-gamma annihilation process, where this lifetime component is well correlated with the void dimension. Based on this principle, one can evaluate the average porosity originating from nanometer size voids, such as free volumes in polymers. It is well documented that the positron annihilation lifetime technique is a powerful tool for characterizing the nanopores of various functional materials. Increased demands on the reliable evaluation of nanopores using this technique have emerged for various industrial applications. This document describes a method for performing positron annihilation lifetime measurements to analyse the lifetime of the ortho-positronium ranging from 1 ns to 10 ns (ascribed to a pore size from approximately 0,3 nm to 1,3 nm in diameter), observed for polymeric materials. It also contains measurement procedures, data analysis, and reporting sections. In the annexes, the results of an interlaboratory comparison using two types of reference materials conducted by eight partic
Scope: This document describes a method for performing positron annihilation lifetime measurements using a 22Na positron source that decays with β+ emission. The β+ (positron) lifetime is determined from a measurement of the lifetime of the ortho-positronium which ranges from 1 ns to 10 ns (ascribed to a pore size from approximately 0,3 nm to 1,3 nm in diameter), as observed for polymeric materials in which the positronium atoms mostly annihilate via a two-gamma annihilation process. This document is not applicable to thin surface layers (that are less than several micrometers). This document does not apply to measuring: — non-positronium forming materials; — positronium-forming materials that induce a spin conversion reaction; — positronium-forming materials that contain chemicals influencing the annihilation process of ortho- positronium by chemical reactions; — positronium-forming materials that contain mesoporous silica gels with a large contribution from the three-gamma annihilation process.